Cause analysis and preventive measures for surface whitening of real stone paint

Release: Common questionsFLAT Official Website

In recent years, when our company surveyed some construction companies and customers, we found that individual walls coated with real stone paint would show one or several small patches of obvious... in rainy or cold weather

In recent years, when our company surveyed some construction companies and customers, we found that a few usersReal stone paintOn painted walls, during rainy or cold weather, one or several small distinct light-colored or white areas different from other parts may appear, especially in the rainy season, and sometimes white also appears where rainwater erodes at downpipe outlets, commonly known as "surface whitening". After fine weather or a rise in temperature, this "surface whitening" phenomenon generally disappears naturally. In some projects, this phenomenon may occasionally appear once, and in others it may recur several times, only disappearing after two years or when the temperature rises. Regarding this phenomenon, the company's technical department consulted many experts and at the same time conducted long-term investigations and a large number of experimental comparisons and sampling studies, and finally identifiedReal stone paintCauses of and solutions for the "surface whitening" phenomenon.


※ Investigations found that the following causes can all lead to the "surface whitening" phenomenon on real stone paint finishes:

1) The primer does not meet the requirements, with high water and vapor permeability, or ordinary latex paint sealer is used instead of primerReal stone paintA dedicated primer, causing moisture in the wall to penetrate into the real stone paint coating; if the intermediate coat of real stone paint is not completely dry and has vitrified, when the external temperature is low or the moisture is high, the moisture inside the real stone paint concentrates and condenses under the topcoat film, causing the surface to turn white;

2) Insufficient wall dryness, low compactness of the plastered surface, or partial omission or non-dense application of the sealing primer causes moisture in the wall to penetrate into the real stone paint coating that has not yet fully vitrified. When the outside temperature is low or the moisture is high, the moisture in the real stone paint condenses under the topcoat film, causing whitening on the surface;

3) Real stone paintIf the temperature is low or the air humidity is too high during spraying, the degree of coating drying and vitrification is low and the moisture content in the coating is too high. In this case, if a topcoat is applied, the moisture in the real stone paint will volatilize more slowly. When the outside temperature is low or the water vapor is high, the moisture in the real stone paint will condense under the topcoat film, causing the surface to turn white, and sometimes the whitened coating will also soften;

4) The use of topcoat that does not meet requirements, poor water resistance of the topcoat, or omissions in application or an insufficient number of coats during topcoat application, which allow external moisture to penetrate, can also cause the surface to turn white;

5) Real stone paintThe formulation system has defects and poor water resistance, which can not only cause large-area surface whitening but even cracking and detachment;

※ In response to the above causes, it is recommended to take the following measures for preventionReal stone paintOccurrence of the "whitening" phenomenon on the facing:

1) Correctly select real stone paint series products; it is recommended to purchase products from regular, professional manufacturers and avoid using low-priced, inferior products from non-professional manufacturers;

2) Do not use latex paint sealer as a substitute for the sealer for real stone paint, because the functional systems of these two products are different. General coatings require the primer to have a certain vapor permeability, whereas the special primer for real stone paint has very low vapor permeability and can isolate most of the moisture in the wall;

3) For walls that are poorly dried or unevenly dried, it is advisable to use an epoxy-series sealing primer, and the application must be thorough and complete, with no skips or missed areas, to increase the barrier against moisture inside the wall;

4) During construction, if the surrounding environment is not easily accessible toReal stone paintCause no pollution; delay the topcoat application as much as possible to increase the drying and curing degree of the real stone paint;

5) Use oil-based resin topcoat or topcoat with high weather resistance as much as possible, and apply it thoroughly and in place to increase protection for the real stone paint and prevent the intrusion of external moisture;

Party and information verification

Party:Guangdong Fulaite Building Materials Co., Ltd. · FLAT. / Company Introduction

When the text involves standards, inspections or material parameters, please verify against the original materials listed in the text and the corresponding product conditions. The original samples and reports can bePage of qualifications and inspection reportConsult; models, batches, and project conditions are different, and relevant data should be confirmed separately.

For engineering cooperation and import and export procurement, you can provide the location, required area and intended texture,Contact FLAT for samples and quotes。

FLAT · Guangdong Fulaite Building Materials Co., Ltd.

Make architecture more beautiful.

Focus on flexible stone (MCM soft stone/soft porcelain), providing texture selection, product information and order production coordination.

Copyright © 2012-2026 Guangdong Fulaite Building Materials Co., Ltd. All Rights Reserved Yue ICP No. 16084041

Headquarters Address:No. 2, West of Tong'an Avenue, Dongfeng Town, Zhongshan City, Guangdong Province
Public Security RecordGuangdong Public Network Security Preparation No. 44200002005257