What are the problems encountered in interior and exterior wall latex paint construction and their solutions?

Release: Common questionsFLAT Official Website

Good or bad results after interior and exterior wall latex paint construction will cause hidden risks in the future. Therefore, in order to avoid unnecessary waste during the initial decoration and increase future costs, knowing the interior and exterior wall latex...

InteriorExterior wall latex paintGood or poor results after construction will both create hidden risks in the future. Therefore, to avoid unnecessary waste during initial decoration and increased future costs, know the relevantExterior wall latex paintCommon questions and solutions.


1. Chalking: If local or large-area chalking occurs shortly after painting, it is caused by the wall surface not being properly treated, the wall putty being too loose, efflorescence, or too much water being added during application.

Treatment method: For wall putty, the loose putty layer must be removed, putty reapplied, one coat of interior and exterior wall sealing primer applied, and then two coats of topcoat. For efflorescence, the powdered part must be cleaned off, and then one coat oflatex paintThe interior and exterior wall sealing primer from the series, followed by two coats of interior and exterior wall paint.


2. InteriorExterior wall latex paintBlistering: blister-like bumps on the surface of the paint film

Cause: moisture penetrates into the paint film, causing the paint layer to lose adhesion; the substrate humidity is too high.
Solution: scrape off the blistered paint surface and use primer

3. InsideExterior wall latex paintWatermarks appear: patches appear on interior and exterior latex paint surfaces, and the color becomes uneven.

Cause: moisture penetration through the exterior wall or pipes; the substrate humidity is too high.
Solution: scrape off the paint surface where patches appear to solve the problem of penetration on exterior walls or pipes

4. Fading and discoloration: the substrate temperature is too high, and water-soluble salt crystals on the wall surface (efflorescence) cause fading and discoloration; fading and discoloration are also caused by excessively strong alkalinity in the substrate, which attacks pigments or resins with weak alkali resistance;

Treatment method: Clean the affected surface thoroughly, neutralize the wall pH with 5%-10% hydrochloric acid, and apply a sealing primer, then apply the weather-resistant elastic exterior wall paint from the latex paint series

5. Sagging: This is caused by applying the paint film too thickly in one coat, a dilution ratio that is too high, or direct application without sanding before the final coat is applied; the paint drips down from above, forming a tear-like or wavy appearance.

Treatment for sagging: increase the number of coats, apply each coat evenly, and pay attention to thin coating; reduce the dilution ratio; for old paint surfaces, sand them flat with sandpaper before coating.

6. Cracking and peeling: poor wall treatment, looseness, alkali content, and construction temperatures that are too low can all cause this; too little coalescent or too little alcohol solvent can also cause it.

Treatment method: Remove the old topcoat on the wall surface where there are cracks or peeling, then re-apply putty and apply one coat.latex paintThe pure eco-friendly alkali-resistant sealing primer from the series, followed by topcoat; the recoat time can be appropriately extended.


7. Shrinkage cavities: This occurs during construction when water, oil, or dust adheres to the application tools or is mixed into the paint, contaminating the coating and causing an uneven paint film surface. This forms a crater-like depression.

How to avoid this situation: the surface must be leveled, and the tools and paint must be kept clean during application.

8. Algae and mold: Algae grow under sun and rain, so buildings need good drainage systems and rainproof facilities. Because rough cement surfaces are porous and tend to retain moisture, they promote algae and mold growth; therefore, for outdoor coating, chooselatex paintThe exterior wall paint from the series; this paint will not damage the original old coating and can adapt to a wide variety of substrates. The coating contains special additives that prevent mold and algae from colonizing, helping to maintain a hygienic environment. The product features ultra-low pollution, broad substrate adaptability, high weather resistance, mold and algae resistance, low odor, and short drying time.

Treatment method: flush the affected area with high-pressure water and assist with manual scraping; after flushing clean, wait until the surface is completely dry, then apply one coat of pure environmentally friendly alkali-resistant sealing primer as a base, and then apply two coats of exterior wall paint to resolve the algae and mold problem.

Party and information verification

Party:Guangdong Fulaite Building Materials Co., Ltd. · FLAT. / Company Introduction

When the text involves standards, inspections or material parameters, please verify against the original materials listed in the text and the corresponding product conditions. The original samples and reports can bePage of qualifications and inspection reportConsult; models, batches, and project conditions are different, and relevant data should be confirmed separately.

For engineering cooperation and import and export procurement, you can provide the location, required area and intended texture,Contact FLAT for samples and quotes。

FLAT · Guangdong Fulaite Building Materials Co., Ltd.

Make architecture more beautiful.

Focus on flexible stone (MCM soft stone/soft porcelain), providing texture selection, product information and order production coordination.

Copyright © 2012-2026 Guangdong Fulaite Building Materials Co., Ltd. All Rights Reserved Yue ICP No. 16084041

Headquarters Address:No. 2, West of Tong'an Avenue, Dongfeng Town, Zhongshan City, Guangdong Province
Public Security RecordGuangdong Public Network Security Preparation No. 44200002005257