Real stone paint construction process
Level the surface → spray the sealing primer → mark the joint layout with chalk lines → apply two layers of masking tape → spray coat 1 of natural stone coating → remove masking-tape layer 1 → spray coat 2 of natural stone coating → remove masking-tape layer 2 → finish the joints → apply 2 coats of clear protective finish.
Real stone paintQuality control
1. Use small-particle real stone paint. After spraying, the surface is required to be flat with small undulations, and the particles are evenly distributed, dense, and consistent in color.
2. The mortar joints must be horizontal and vertical, with consistent width; pay particular attention when peeling off the dividing strips not to pull off the underlying coating.
3. For all external corners, the long side should face the short side during layout, giving the visual effect of whole-brick masonry.
4. For dividing tape, paper-faced tape should be used; the paper side should faceReal stone paintIt has good adsorption; if plastic-faced tape is used, it will cause the real stone paint to run. At the same time, when constructing in summer, the tape is required to have good temperature resistance, to avoid the tape backing melting at slightly higher temperatures, which would make the tape difficult to tear off.
5. Grasp the timing of tearing off the masking tape. When the surface of the real stone paint is dry and shows no obvious indentation when pressed by hand and is not sticky to the touch, it can be torn off. Tearing off too early will causeReal stone paintSagging; if the tape is peeled off too late, first, the masking tape is difficult to remove, and second, it will cause the real stone paint at the mortar joints to be peeled off, making the mortar joints uneven.
6. Of the same monomerReal stone paintYes, purchase the full quantity in one go to reduce color differences.
Some friends find that after completing a real stone paint project, some areas of the real stone paint will become mottled and whitish. What causes this problem? The reasons are,
I and preparationReal stone paintIt has a great deal to do with the emulsion used. Some emulsion manufacturers, in order to increase the stability of the emulsion, use excessive amounts of surfactant, which leads to a decrease in the water resistance of the emulsion.
Two,Real stone paintTo save costs, some manufacturers add only a small amount of emulsion, which makes the real stone paint film loose and not dense enough after drying; the film has a higher water absorption rate and lower bonding strength. Once prolonged rainy weather occurs, rainwater gradually penetrates into the paint film, causing the real stone paint film to whiten. Third, some real stone paint manufacturers add large amounts of thickeners such as hydroxymethyl cellulose and hydroxyethyl cellulose during preparation, and these substances are water-soluble or hydrophilic; after the real stone paint forms a film, they remain in the coating and reduce the coating's water resistance.
Therefore, avoidReal stone paintFor mottling, ultimately what matters is still choosing a good real stone paint manufacturer and choosing a real stone paint brand with many years of production experience to control product quality. For example, Wanlei real stone paint started making real stone paint early on; after more than 10 years of research and development, it has continuously launched new real stone paint products and improved the real stone paint system, giving Wanlei real stone paint better and more stable quality and better workability. FLAT's new-formula resistance-free real stone paint is even nationwide, bringing a new chapter to the real stone paint industry.
Text by Zhongshan CityFLATBuilding Materials Co., Ltd. (http://www.zsfulaite.com/). If reproduced, please indicate the source.