Uneven color after real stone paint completion? Discoloration? What is the cause

Release: Corporate NewsFLAT Official Website

Analysis of the causes of uneven color in real stone paint: 1. Construction problems: uneven spraying leads to uneven hiding power and can also easily cause uneven color; when real stone paint in two colors is applied in cross operations,...


Real stone paintCause analysis of mottling:

1. Application problems: Uneven spraying leads to uneven hiding power and is also prone to causing color mottling;Real stone paintWhen two colors are being applied in cross-over operations, protection is mandatory; otherwise, they can easily contaminate each other and cause uneven color.


2、Real stone paintPrimer problems: no primer applied (or workmanship cut during application). Water-based alkali-resistant primer can effectively prevent efflorescence and salt precipitation on the topcoat, and clear primer for real stone paint can effectively reduce uneven color in real stone paint. Clear alkali-resistant primer can effectively preventReal stone paintThe efflorescence and blooming problem of real stone paint caused by white crystals appearing due to alkali efflorescence and salt efflorescence on the topcoat.

3. Problems with the topcoat: when rolling on the topcoat, it must be rolled evenly and must not sag; minimize overlaps and avoid rolling too thickly in some areas, which would cause excessively high gloss and lead to color variation due to differing gloss.


4. Construction condition issues: During construction, the suitable temperature is 5~30°C; the humidity is 50%~70%, and there should be no wind or little wind. In windy weather, it is difficult to spray evenly and easy to cause blooming. Too low a temperature and too high a humidity will affect the drying speed, thereby affecting film formation, and abnormal coating film appearance is likely to occur, thus causing blooming.


5. The issue of water addition: real stone paint is diluted with water; adding too much water makes it prone to sagging and tear marks, and causes the emulsion to float, resulting in localized whitening and easily leading to color unevenness.

6. Air pressure issues: unstable air pressure causes uneven film thickness, leading to mottling; excessive air pressure makes the film flat and fine, with small, dense dots and greater material loss; insufficient air pressure gives the film a strong textured feel and may even cause pinholes, with the film showing sagging.


7. Batch issues: Real stone paint from the same batch should be applied to the same wall surface, preferably with dividing joints, and each divided section should be completed in a single application; the dew point temperatures of the substrates on the same application surface should be similar; the primer should have no missed spots, and the gloss should be basically consistent.

The above is what the editor has compiled for you.Real stone paintRegarding the causes of uneven color after construction, you can check whether any of the construction-related issues listed apply. You are welcome to raise more various difficult problems encountered during construction!

Party and information verification

Party:Guangdong Fulaite Building Materials Co., Ltd. · FLAT. / Company Introduction

When the text involves standards, inspections or material parameters, please verify against the original materials listed in the text and the corresponding product conditions. The original samples and reports can bePage of qualifications and inspection reportConsult; models, batches, and project conditions are different, and relevant data should be confirmed separately.

For engineering cooperation and import and export procurement, you can provide the location, required area and intended texture,Contact FLAT for samples and quotes。

FLAT · Guangdong Fulaite Building Materials Co., Ltd.

Make architecture more beautiful.

Focus on flexible stone (MCM soft stone/soft porcelain), providing texture selection, product information and order production coordination.

Copyright © 2012-2026 Guangdong Fulaite Building Materials Co., Ltd. All Rights Reserved Yue ICP No. 16084041

Headquarters Address:No. 2, West of Tong'an Avenue, Dongfeng Town, Zhongshan City, Guangdong Province
Public Security RecordGuangdong Public Network Security Preparation No. 44200002005257